当前位置: X-MOL 学术Int. J. Self-Propag. High-Temp. Synth. › 论文详情
Our official English website, www.x-mol.net, welcomes your feedback! (Note: you will need to create a separate account there.)
Ti–TiC Composites by Thermal Explosion in Mechanically Activated Ti–xC Powder Blends (x = 1.0–6.3 wt %)
International Journal of Self-Propagating High-Temperature Synthesis ( IF 0.5 ) Pub Date : 2021-06-30 , DOI: 10.3103/s1061386221020102
G. A. Pribytkov , A. V. Baranovskiy , I. A. Firsina , V. V. Korzhova , M. G. Krinitcyn , E. N. Korosteleva

Abstract

Warmup of mechanically activated Ti–xC powder mixtures (x = 1.0, 2.1, 4.2, and 6.3 wt %) in a furnace preheated to 800°C was found to result in thermal explosion (volume reaction) in mixtures with x = 4.2 and 6.3 wt %. Activated powder mixtures and combustion products were characterized by XRD, optical metallography, and SEM/EDX. Combustion products represented metal-matrix Ti–TiC composites containing different amounts of strengthening agent. Our results may turn interesting to those engaged in deposition (cladding) of protective Ti–TiC coatings using reactive Ti–C mechanocomposites as a starting material.



中文翻译:

在机械活化的 Ti-xC 粉末混合物中通过热爆炸制备 Ti-TiC 复合材料(x = 1.0-6.3 wt %)

摘要

发现在预热至 800°C 的炉子中加热机械活化的 Ti– x C 粉末混合物(x = 1.0、2.1、4.2 和 6.3 wt%)会导致x = 4.2 和6.3 重量%。活化的粉末混合物和燃烧产物通过 XRD、光学金相和 SEM/EDX 进行表征。燃烧产物代表含有不同量增强剂的金属基体 Ti-TiC 复合材料。我们的结果可能会对那些使用反应性 Ti-C 机械复合材料作为起始材料来沉积(包覆)保护性 Ti-TiC 涂层的人感兴趣。