当前位置: X-MOL 学术J. Mater. Cycles Waste Manag. › 论文详情
Our official English website, www.x-mol.net, welcomes your feedback! (Note: you will need to create a separate account there.)
Devulcanized EPDM without paraffinic oil in the production of blends as a potential application of the residues from automobile industry
Journal of Material Cycles and Waste Management ( IF 2.7 ) Pub Date : 2019-11-05 , DOI: 10.1007/s10163-019-00938-x
Fabiula D. B. de Sousa , Aline Zanchet , Elaine S. Marczynski , Vinicius Pistor , Rudinei Fiorio , Janaina S. Crespo

Vulcanized residues of ethylene–propylene–diene monomer rubber (EPDM) from expanded profiles trims, called EPDM-r, were treated to remove the paraffinic oil and then devulcanized by microwaves at different exposure times (0, 2, 3 and 4 min). Elastomeric formulations of EPDM-r compound/raw EPDM compound containing 67 wt% of recycled phase were produced, and the characteristics of the vulcanization process, mechanical and dynamic-mechanical properties, morphology and accelerated aging of the blends were analyzed. The promising results showed that it is possible to obtain new rubber compositions containing 67 wt% of EPDM-r with similar—or even higher—mechanical properties than the Reference sample (without EPDM-r), pointing out to the potential use of devulcanized EPDM-r in several applications, as a possible solution to the destination of these materials, aiming at the sustainable development.

中文翻译:

不含石蜡油的脱硫EPDM在共混物中的生产,可作为汽车工业残留物的潜在用途

对膨胀型饰条中被称为EPDM-r的乙烯-丙烯-二烯单体橡胶(EPDM)的硫化残留物进行处理,以去除石蜡油,然后在不同的暴露时间(0、2、3和4分钟)通过微波进行脱硫。制备了包含67 wt%循环相的EPDM-r化合物/原始EPDM化合物的弹性体配方,并分析了硫化过程的特性,机械和动态机械性能,混合物的形态和加速老化。令人鼓舞的结果表明,有可能获得含有67 wt%EPDM-r的新橡胶组合物,其力学性能与参考样品(不含EPDM-r)相似或什至更高,指出了硫化EPDM的潜在用途-r在几个应用程序中,