Solid Electrolyte Interface in Zn-Based Battery Systems
Nano-Micro Letters ( IF 31.6 ) Pub Date : 2022-10-19 , DOI: 10.1007/s40820-022-00939-w Xinyu Wang 1 , Xiaomin Li 1 , Huiqing Fan 2 , Longtao Ma 1
中文翻译:
锌基电池系统中的固体电解质界面
更新日期:2022-10-20
Nano-Micro Letters ( IF 31.6 ) Pub Date : 2022-10-19 , DOI: 10.1007/s40820-022-00939-w Xinyu Wang 1 , Xiaomin Li 1 , Huiqing Fan 2 , Longtao Ma 1
Affiliation
-
The formation mechanism of solid electrolyte interface (SEI) is analyzed based on charge distributions at the electrode/electrolyte interface and molecular orbital theory.
-
The factors affecting the formation of SEI are generalized from four aspects: Zn anode, electrolyte, current density and temperature.
-
The design strategies for SEI layer are proposed from regulating temperature, electric and magnetic fields.