Influence on off-gassing during storage of Scots pine wood pellets produced from sawdust with different extractive contents
Biomass & Bioenergy ( IF 5.8 ) Pub Date : 2021-12-11 , DOI: 10.1016/j.biombioe.2021.106325
Workson Siwale 1, 2 , Stefan Frodeson 1 , Jonas Berghel 1 , Gunnar Henriksson 3 , Michael Finell 4 , Mehrdad Arshadi 4 , Carina Jonsson 4
Affiliation  

Off-gassing and self-heating are the major challenges when it comes to transportation and storage of wood pellets. The heat generated due to self-heating poses a fire risk while off-gassing of toxic gasses such as carbon monoxide (CO) and some volatile organic compounds (VOCs) is an environmental and human health risk. With the increase in production volumes of wood pellets which has subsequently increased the amounts of wood pellets in transportation and storage, there is need to find lasting solutions to off-gassing and self-heating of wood pellets. The objective of this study was to test the off-gassing abilities of Scots pine wood pellets produced from sawdust with varying amounts of extractives. The aim is to come up with raw material pre-treatment measures so as to produce wood pellets that are not liable to off-gassing. Six (6) types of sawdust raw materials namely; fresh pine sawdust (FPS), stored pine sawdust (SPS), sawdust plus pine rosin (PRS), sawdust plus linseed oil (LOS), sawdust plus tall oil (TOS) and acetone extracted sawdust (AES) were used to produce the pellets. The produced pellets were then subjected to off-gassing tests under controlled conditions using the ECOM J2KN analyser. The concentrations of carbon monoxide, carbon dioxide and methane increased with storage time but slowed down towards the end of the nine days test period. The formation of these gasses were largely dependent on the type of extractives present in the raw material and not the total extractive content. The formation of methane started later than the other gases and coincided with the time when residual oxygen was depleted.



中文翻译:

不同提取物含量的锯末生产的赤松木颗粒对储存过程中脱气的影响

在木屑颗粒的运输和储存方面,排气和自加热是主要挑战。由于自热产生的热量会带来火灾风险,而一氧化碳 (CO) 和一些挥发性有机化合物 (VOC) 等有毒气体的排放则对环境和人类健康构成威胁。随着木屑颗粒产量的增加,随后增加了运输和储存中木屑颗粒的数量,需要找到木屑颗粒脱气和自热的持久解决方案。本研究的目的是测试由含有不同提取物数量的锯末生产的苏格兰松木颗粒的除气能力。目的是提出原料预处理措施,以生产不易脱气的木屑颗粒。六 (6) 种锯末原料即;使用新鲜松木屑 (FPS)、储存松木屑 (SPS)、木屑加松香 (PRS)、木屑加亚麻籽油 (LOS)、木屑加妥尔油 (TOS) 和丙酮提取的木屑 (AES) 来生产颗粒. 然后使用 ECOM J2KN 分析仪在受控条件下对生产的颗粒进行排气测试。一氧化碳、二氧化碳和甲烷的浓度随着储存时间的增加而增加,但在 9 天测试期结束时减慢。这些气体的形成很大程度上取决于原材料中存在的提取物的类型,而不是提取物的总含量。甲烷的形成开始于其他气体,并且与剩余氧气耗尽的时间一致。使用储存的松木屑 (SPS)、木屑加松香 (PRS)、木屑加亚麻籽油 (LOS)、木屑加妥尔油 (TOS) 和丙酮提取的木屑 (AES) 来生产颗粒。然后使用 ECOM J2KN 分析仪在受控条件下对生产的颗粒进行排气测试。一氧化碳、二氧化碳和甲烷的浓度随着储存时间的增加而增加,但在 9 天测试期结束时减慢。这些气体的形成很大程度上取决于原材料中存在的提取物的类型,而不是提取物的总含量。甲烷的形成开始于其他气体,并且与剩余氧气耗尽的时间一致。使用储存的松木屑 (SPS)、木屑加松香 (PRS)、木屑加亚麻籽油 (LOS)、木屑加妥尔油 (TOS) 和丙酮提取的木屑 (AES) 来生产颗粒。然后使用 ECOM J2KN 分析仪在受控条件下对生产的颗粒进行排气测试。一氧化碳、二氧化碳和甲烷的浓度随着储存时间的增加而增加,但在 9 天测试期结束时减慢。这些气体的形成很大程度上取决于原材料中存在的提取物的类型,而不是提取物的总含量。甲烷的形成开始于其他气体,并且与剩余氧气耗尽的时间一致。木屑加妥尔油 (TOS) 和丙酮提取的木屑 (AES) 用于生产颗粒。然后使用 ECOM J2KN 分析仪在受控条件下对生产的颗粒进行排气测试。一氧化碳、二氧化碳和甲烷的浓度随着储存时间的增加而增加,但在 9 天测试期结束时减慢。这些气体的形成很大程度上取决于原材料中存在的提取物的类型,而不是提取物的总含量。甲烷的形成开始于其他气体,并且与剩余氧气耗尽的时间一致。木屑加妥尔油 (TOS) 和丙酮提取的木屑 (AES) 用于生产颗粒。然后使用 ECOM J2KN 分析仪在受控条件下对生产的颗粒进行排气测试。一氧化碳、二氧化碳和甲烷的浓度随着储存时间的增加而增加,但在 9 天测试期结束时减慢。这些气体的形成很大程度上取决于原材料中存在的提取物的类型,而不是提取物的总含量。甲烷的形成开始于其他气体,并且与剩余氧气耗尽的时间一致。二氧化碳和甲烷随着储存时间的增加而增加,但在 9 天测试期结束时减慢。这些气体的形成很大程度上取决于原材料中存在的提取物的类型,而不是提取物的总含量。甲烷的形成开始于其他气体,并且与剩余氧气耗尽的时间一致。二氧化碳和甲烷随着储存时间的增加而增加,但在 9 天测试期结束时减慢。这些气体的形成很大程度上取决于原材料中存在的提取物的类型,而不是提取物的总含量。甲烷的形成开始于其他气体,并且与剩余氧气耗尽的时间一致。