Magnetic Properties and Domain Structure of Alloy Sm(Co, Fe, Cu, Zr)7.5 in Different Stages of Heat Treatment
Metal Science and Heat Treatment ( IF 0.6 ) Pub Date : 2021-08-10 , DOI: 10.1007/s11041-021-00660-2
A. S. Lileev 1 , Yu. V. Konyukhov 1
Affiliation  

The magnetic properties and the changes in the domain structure of alloy Sm(Co, Fe, Cu, Zr)7.5 are studied after different variants of heat treatment, i.e. (1) quenching from 1200°C with cooling in a helium jet; (2) quenching and tempering at 800°C for 16 h, cooling at a rate of 50 K/min to room temperature; and (3) quenching, tempering at 800°C for 16 h, and cooling at a rate of 1.7 K/min. The influence of the heat treatment modes on the coercivity and the domain sizes is determined. The mechanism of variation of these characteristics is analyzed.



中文翻译:

Sm(Co, Fe, Cu, Zr)7.5合金不同热处理阶段的磁性能和畴结构

研究了合金 Sm(Co, Fe, Cu, Zr) 7.5在不同热处理变体后的磁性能和畴结构的变化,即 ( 1 ) 从 1200°C 淬火并在氦射流中冷却;( 2 )800℃调质16h,以50K/min的速度冷却至室温;( 3 )淬火,800℃回火16h,以1.7K/min的速度冷却。确定热处理模式对矫顽力和畴尺寸的影响。分析了这些特性的变化机制。