当前位置: X-MOL 学术J. Thermoplast. Compos. Mater. › 论文详情
Our official English website, www.x-mol.net, welcomes your feedback! (Note: you will need to create a separate account there.)
Effect of macro and molecular initiators on the structure-property relationship of poly(ε-caprolactone)
Journal of Thermoplastic Composite Materials ( IF 3.6 ) Pub Date : 2021-07-05 , DOI: 10.1177/08927057211027196
A Thamizhlarasan, B Meenarathi, R Anbarasan

Ring opening polymerization (ROP) of ε-caprolactone (CL) was carried out by bulk polymerization technique using stannous octoate (SO) as a catalyst and in the presence of macro or molecular initiator for 5 h under inert atmosphere with mild stirring. The % yield of poly(ε-caprolactone) (PCL) obtained was calculated and compared based on the chemical structure of macro and molecular initiators. Various analytical techniques such as FT-IR, 1H-NMR, XPS, GPC, DSC, TGA, SEM and WCA were used to characterize the PCL. The FT-IR spectrum showed the C=O stretching around ∼1725 cm−1. The aromatic proton signal of isoeugenol (IE) initiator appeared at 7–8 ppm in the proton NMR spectrum. The experimental results obtained were compared with the literature values.



中文翻译:

大分子和分子引发剂对聚(ε-己内酯)结构性能关系的影响

ε-己内酯(CL)的开环聚合(ROP)是通过本体聚合技术进行的,使用辛酸亚锡(SO)作为催化剂,在大分子或分子引发剂的存在下,在惰性气氛下温和搅拌5小时。基于宏观和分子引发剂的化学结构计算和比较获得的聚(ε-己内酯)(PCL)的%产率。使用各种分析技术,如 FT-IR、1 H-NMR、XPS、GPC、DSC、TGA、SEM 和 WCA 来表征 PCL。FT-IR 光谱显示 C=O 拉伸约 1725 cm -1。异丁香酚 (IE) 引发剂的芳香质子信号出现在质子核磁共振谱中的 7-8 ppm。获得的实验结果与文献值进行了比较。