In the present work, two different hardfacings, namely SZ (Super-Zed alloy; C3.83Cr33.37) and ZK (Zedalloy-K; C0.65Cr4.5Mo8.18) were deposited on EN-47 ploughshare steel by manual metal arc welding process to enhance the abrasive wear resistance. In addition, the influence of heat-treatment of steel by two different methods, i.e., carburizing (C) and through-hardening (Q&T), on the abrasive wear behaviour has also been investigated. Abrasive wear studies were conducted on bare, hardfaced, and heat-treated steel in a laboratory by using a three-body dry sand rubber wheel test rig as per the ASTM G-65 standard. The bare steel suffered a high wear rate, which may be attributed to its soft ferritic-pearlitic microstructure. The abrasive wear rate of tested specimens was found to be 1.7651 × 10 −3 g m −1 , 0.7439 × 10 −3 g m −1 , 0.961 × 10 −3 g m −1 , 0.992 × 10 −3 g m −1 and 1.21 × 10 −3 g m<...

中文翻译:

耕作应用的EN-47硬面和热处理钢的摩擦学性能

在目前的工作中,通过手工金属电弧焊在EN-47犁ough钢上沉积了两种不同的堆焊层,即SZ(超Zed合金; C3.83Cr33.37)和ZK(Zedalloy-K; C0.65Cr4.5Mo8.18)。焊接过程中增强了耐磨性。另外,还研究了通过两种不同的方法(即渗碳(C)和直通淬火(Q&T))对钢进行热处理对磨料磨损行为的影响。使用ASTM G-65标准的三体干砂橡胶轮试验装置,在实验室中对裸露,硬面和热处理的钢进行磨料磨损研究。裸钢具有较高的磨损率,这可能归因于其软的铁素体-珠光体显微组织。发现测试样品的磨料磨损率为1.7651  ×  10 -3 gm -1,0.7439 ×  10 -3 gm -1,0.961  ×  10 -3 gm -1,0.992  ×  10 -3 gm -1和1.21 ×  10 -3 gm  <...
更新日期:2020-10-06
down
wechat
bug