当前位置: X-MOL 学术Russ. J. Nondestruct. Test. › 论文详情
Our official English website, www.x-mol.net, welcomes your feedback! (Note: you will need to create a separate account there.)
Performance Evaluation of 42 mm Diameter Stranded Ungalvanised Haulage Rope in a Mono-Cable Passenger Ropeway
Russian Journal of Nondestructive Testing ( IF 0.9 ) Pub Date : 2020-10-01 , DOI: 10.1134/s1061830920070025
Debasish Basak

Abstract

Most common conventional method of rope condition evaluation is visual method i.e. watching the exterior strand and outer surface only. Core damage cannot be detected. To assess the rope condition, magnetic nondestructive method is the most suitable method. Periodic rope assessment is necessary to prevent rope failures and extension of rope life. Flaw detectors in the Magnetic Rope Tester detect LMA (loss in metallic area) and LF (localized faults) [1, 2]. This paper describes the performance of a haulage rope in two years.



中文翻译:

单芯索道42 mm直径绞合镀锌牵引索的性能评估

摘要

绳索状态评估的最常见常规方法是视觉方法,即仅观察外部绳股和外部表面。无法检测到核心损坏。要评估绳索状况,最适合使用磁性无损检测方法。定期进行绳索评估对于防止绳索故障和延长绳索寿命是必要的。磁力绳测试仪中的缺陷检测器可检测LMA(金属区域的损耗)和LF(局部故障)[1、2]。本文介绍了牵引绳在两年内的性能。