Dephosphorization of high silicon hot metal based on double slag converter steelmaking technology
Ironmaking & Steelmaking ( IF 1.7 ) Pub Date : 2020-09-22 , DOI: 10.1080/03019233.2020.1807288 Yuxiang Dai 1 , Jing Li 1 , Chengbin Shi 1 , Wei Yan 1
Ironmaking & Steelmaking ( IF 1.7 ) Pub Date : 2020-09-22 , DOI: 10.1080/03019233.2020.1807288 Yuxiang Dai 1 , Jing Li 1 , Chengbin Shi 1 , Wei Yan 1
Affiliation
The average silicon content of the hot metal produced by Corex furnace is 0.6–1.5 mass%, which increases the oxygen blowing time and leads the unsatisfactory dephosphorization, high reblowing rate....
中文翻译:
基于双渣转炉炼钢技术的高硅铁水脱磷
Corex炉生产的铁水平均硅含量为0.6-1.5%,增加了吹氧时间,导致脱磷效果不理想,重吹率高....