New self‐healing crosslinked bisphenol‐S polyurethane (BPS/PU) including thermal reversible urethane bonds is prepared to balance the mechanical and self‐healing properties. BPS/PU is synthesized with BPS as chain extender to improve the mechanical property in the effect of high molecular regularity of BPS and extra stronger physical crosslinking in BPS/PU. The crosslinked structure of BPS/PU is confirmed by Fourier transform infrared spectra and swelling‐dissolution test. BPS/PU demonstrates great thermal reversability after three heating and cooling cycles and exhibits shorter relaxation time (3.3 min). The tensile strength and the tensile elongation of BPS/PU are up to 14.54 MPa and 877.12%, respectively, which are much higher than the value reported in literature. The qualitative self‐healing analysis of BPS/PU confirms that the cracks can be healed largely after healing progress, and the quantitative self‐healing analysis exhibits great healing properties with the healing efficiency of up to 77.92%.

中文翻译:

基于封端和解封反应的热可逆交联聚氨酯

包括热可逆氨基甲酸酯键在内的新型自修复交联双酚S聚氨酯(BPS / PU)可以平衡机械和自修复性能。BPS / PU以BPS为扩链剂合成,以改善BPS的高分子规则性和BPS / PU中更强的物理交联效果的机械性能。BPS / PU的交联结构通过傅立叶变换红外光谱和溶胀溶解测试得到证实。在三个加热和冷却循环后,BPS / PU表现出出色的热可逆性,并且松弛时间更短(3.3分钟)。BPS / PU的拉伸强度和拉伸伸长率分别高达14.54 MPa和877.12%,远高于文献报道的值。