Abstract The purpose of the research was to establish the influence of the solution composition and the electrophoretic deposition voltage on the coating homogeneity and thickness, nanohardness, adhesion, corrosion resistance and wettability. The Ti13Zr13Nb alloy was coated by the electrophoretic technique with hydroxyapatite in a solution containing 0.1, 0.2 or 0.5 g nanoHAp in 100 mL of suspension and at voltage 15, 30 or 50 V. The scanning electron and atomic force microscopies, polarization curves technique for corrosion assessment, nanoindentation and nanoscratch tests, and measurements of contact angle in simulated body fluid were performed. The obtained results revealed the complex and interrelated effects of both process determinants on the structure and properties of hydroxyapatite coatings, which were attributed to the role of the size, shape and content in suspension of hydroxyapatite particles.

中文翻译:

溶液组成和电泳沉积电压对Ti13Zr13Nb合金纳米羟基磷灰石涂层各种性能的影响

摘要 本研究的目的是确定溶液组成和电泳沉积电压对涂层均匀性和厚度、纳米硬度、附着力、耐腐蚀性和润湿性的影响。Ti13Zr13Nb 合金在 100 mL 悬浮液中含有 0.1、0.2 或 0.5 g nanoHAp,电压为 15、30 或 50 V,通过电泳技术用羟基磷灰石涂覆。 扫描电子和原子力显微镜,极化曲线技术用于腐蚀进行了评估、纳米压痕和纳米划痕测试以及模拟体液中接触角的测量。获得的结果揭示了两种工艺决定因素对羟基磷灰石涂层的结构和性能的复杂和相互关联的影响,这归因于尺寸的作用,