近期论文
查看导师新发文章
(温馨提示:请注意重名现象,建议点开原文通过作者单位确认)
代表性同行评审期刊论文
[1] P. Dou*, Z.X. Xin, W. Sang, A. Kimura, Age-hardening mechanisms of 15Cr ODS ferritic steels with 5, 7 and 9 wt.% Al at 475 °C for 9000 h, Journal of Nuclear Materials, In press, (Corresponding Author) (JCR一区).
[2] W. Sang, P. Dou*, A. Kimura, Early-stage thermal ageing behavior of 12Cr, 12Cr–7Al and 18Cr–9Al ODS steels, Journal of Nuclear Materials, 534(2020)152164, (Corresponding Author) (JCR一区).
[3] P. Dou*, W. Sang, A. Kimura, Effects of the contents of Al, Ti, W and Y2O3 on long-term thermal ageing behavior of 15Cr ODS ferritic steels, Journal of Nuclear Materials, 534(2020)152129 (Corresponding Author) (JCR一区).
[4] P. Dou*, Q. Ye, A. Kimura, Crystal and metal/oxide interface structures of nanoparticles in 15Cr–2W–0.1Ti–4Al–0.6Hf–0.35Y2O3 ODS steel, Journal of Nuclear Materials, 533(2020)152029 (Corresponding Author) (JCR一区).
[5] P. Dou*, S.M. Jiang, L.L. Qiu, A. Kimura, Effects of contents of Al, Zr and Ti on oxide particles in Fe–15Cr–2W–0.35Y2O3 ODS steels, Journal of Nuclear Materials, 531(2020)152025 (Corresponding Author) (JCR一区).
[6] P. Song, A. Kimura, K. Yabuuchi, P. Dou, H. Watanabe, J. Gao, Y.J. Huang, Assessment of phase stability of oxide particles in different types of 15Cr–ODS ferritic steels under 6.4 MeV Fe ion irradiation at 200 °C, Journal of Nuclear Materials, 529(2020)151953. (JCR一区)
[7] P. Dou*, L.L. Qiu, S.M. Jiang, A. Kimura, Crystal and Metal/oxide Interface Structures of Nanoparticles in Fe–16Cr–0.1Ti–0.35Y2O3 ODS steel, Journal of Nuclear Materials, 523(2019)320–332 (Corresponding Author) (JCR一区).
[8] P. Dou*, W. Sang, A. Kimura, Morphology, Crystal and Metal/oxide Interface Structures of Nanoparticles in Fe–15Cr–2W–0.5Ti–7Al–0.4Zr–0.5Y2O3 ODS steel, Journal of Nuclear Materials, 523(2019)231–247 (Corresponding Author) (JCR一区).
[9] P. Dou*, X.W. Yuan, P.P. Jin, L.L. Qiu, A. Kimura, S. Ukai, Effect of Ti Content on Oxide Particles in Fe–Cr ODS steels, Materials Science, (Accepted) (Corresponding Author).
[10] P. Dou*, Y.T. Zhang, Y. Fang, Q. Ye, A. Kimura, S. Ukai, EFTEM Study on the Effect of Al Content on the Phase Separation Behavior in 18Cr–ODS Steels, Materials Science, 8(9) (2018) 917–927 (Corresponding Author).
[11] P. Dou*, A. Kimura, R. Kasada, T. Okuda, M. Inoue, S. Ukai, S. Ohnuki, T. Fujisawa, F. Abe, S. Jiang, Z.G Yang, TEM and HRTEM Study of Oxide Particles in an Al-alloyed High–Cr Oxide Dispersion Strengthened Steel with Hf Addition, Journal of Nuclear Materials, 485(2017)189–201 (Corresponding Author) (JCR一区).
[12] Z.J. Wang, C.T. Liu, P. Dou, Thermodynamics of Vacancies and Clusters in High-entropy Alloys, Physical Review Materials, 043601, 2017, 1–5.
[13] P. Dou*, X. Zhang, A. Kimura, Y.H. He, C.T. Liu, Effects of Zr and Ti Contents on Oxide Nanoparticles in Al-alloyed High-Cr ODS Steels, Materials Science, 7(2017)413–422 (Corresponding Author).
[14] P. Dou*, A. Kimura, R. Kasada, T. Okuda, M. Inoue, S. Ukai, S. Ohnuki, T. Fujisawa, F. Abe, TEM and HRTEM Study of Oxide Particles in an Al-alloyed High–Cr Oxide Dispersion Strengthened Steel with Zr Addition, Journal of Nuclear Materials, 444 (2013) 441–453 (Corresponding Author) (JCR一区).
[15] P. Dou*, A. Kimura, R. Kasada, T. Okuda, M. Inoue, S. Ukai, S. Ohnuki, T. Fujisawa, F. Abe, Effects of Titanium Concentration and Tungsten Addition on the Nano-Mesoscopic Structure of High–Cr Oxide Dispersion Strengthened (ODS) Ferritic Steels, Journal of Nuclear Materials,442 (2013) S95–S100 (Corresponding Author) (JCR一区).
[16] P. Dou*, A. Kimura, T. Okuda, M. Inoue, S. Ukai, S. Ohnuki, T. Fujisawa, F. Abe, Polymorphic and Coherency Transition of Y–Al Complex Oxide Particles with Extrusion Temperature in an Al-alloyed High–Cr Oxide Dispersion Strengthened Ferritic Steel, Acta Materialia, 59 (2011) 992–1002 (Corresponding Author) (JCR一区).
[17] P. Dou*, A. Kimura, T. Okuda, M. Inoue, S. Ukai, S. Ohnuki, T. Fujisawa, F. Abe, Effects of Extrusion Temperature on the Nano-Mesoscopic Structure and Mechanical Properties of High–Cr ODS Ferritic Steel, Journal of Nuclear Materials, 417 (2011) 166–170 (Corresponding Author) (JCR一区).
[18] P. Dou*, R. Kasada, Preliminary Study on Nano- and Micro-Composite Sol–Gel Based Alumina Coatings on Structural Components of Lead–Bismuth Eutectic Cooled Fast Breeder Reactors, Journal of Nuclear Materials, 409 (2011) 177–182 (Corresponding Author) (JCR一区).
[19] R. Kasada, P. Dou, Sol–Gel Composite Coatings as Anti-Corrosion Barrier for Structural Materials of Lead-Bismuth Eutectic Cooled Fast Reactor, Journal of Nuclear Materials, 2013, 440, 647–653 (JCR一区).
[20] N.Y. Iwata, T. Liu, P. Dou*, R. Kasada, A. Kimura, T. Okuda, M. Inoue, F. Abe, S. Ukai, S. Ohnuki, T. Fujisawa, Effects of MA Environment on the Mechanical and Microstructural Properties of ODS Ferritic Steels, Journal of Nuclear Materials, 417 (2011) 162–165 (JCR一区).
[21] A. Kimura, R. Kasada, N. Iwata, H. Kishimoto, C.H. Zhang, J. Isselin, P. Dou, J.H. Lee, N. Muthukumar, T. Okuda, M. Inoue, S. Ukai, S. Ohnuki, T. Fujisawa, T. F. Abe, Development of Al-Added high–Cr ODS steels for Fuel Cladding of Next Generation Nuclear Systems, Journal of Nuclear Materials, 417 (2011) 176–179 (JCR一区).
[22] P. Dou*, S.F. Suo, Z.G. Yang, Y.G. Li, D.R. Chen, Ratcheting Short Crack Behavior in Medium Carbon Bainitic Back-up Roll Steel under Mild Tractive Rolling Contact, Wear 268 (2010) 302–308, (Corresponding Author) (JCR一区).
[23] P. Dou*, S.F. Suo, B.Z. Bai, Z.G. Yang, Y.G. Li, Vertical Short Crack Initiation in Medium Carbon Bainitic Steel under Mild Tractive Rolling Contact, Journal of Iron and Steel Research International, 15(3) (2008) 37–41, (Corresponding Author).
[24] P. Dou*, X.H. Jia, S.F. Suo, R.C. Wang, M. Zhang, Pressure Distribution at the Stump/socket Interface in Transtibial Amputees during Walking on Stairs, Slope and Non-flat Road, Clinical Biomechanics, 21 (2006) 1067–1073, (Corresponding Author) (JCR一区).
[25] Y.G. Li, G.Z. Kang, C.A. Wang, P. Dou, J. Wang, Vertical Short-crack Behavior and its Application in Rolling Contact Fatigue, International Journal of Fatigue, 28 (2006) 804–811 (JCR一区).
[26] P. Dou*, Y.G. Li, K.M. Liang, Behavior of Short Fatigue Cracks in Medium Carbon Bainitic Back-up Roll Steel under Mild Tractive Rolling Contact, Acta Metallurgica Sinica, 41(2) (2005) 140–144, (Corresponding Author).
[27] P. Dou*, Y.G. Li, K.M. Liang, C.A. Wang, Finite Element Analysis of Contact Stresses on the Backup Roll of CVC Hot Rolling Mills, Journal of Tsinghua University (Science and Technology), 45(12) (2005) 1668–1671, (Corresponding Author).
[28] P. Dou*, Y.G. Li, K.M. Liang, B.Z. Bai, Optimization of Preventive Grinding of Backup Roll against Contact Fatigue Cracking, Journal of Iron and Steel Research International, 12(3) (2005) 28–33, 45, (Corresponding Author).
[29] P. Dou*, Y.G. Li, K.M. Liang, B.Z. Bai, Ratcheting Led Surface Failure of Medium Carbon Bainitic Steel under Mild Operation Conditions, Journal of University of Science and Technology Beijing, 12(1) (2005) 60–66, (Corresponding Author).
代表性同行评审技术报告
[1] T. Nozawa and H. Tanigawa, P. Dou, H. Bei, Y. Katoh, L. L. Snead, and R. E. Stoller. Strength and Microstructures of the Fiber/Matrix Interface of Neutron-Irradiated SiC/SiC Composites. Fusion Materials Semiannual Progress Report, DOE–ER–0313/51; 2012.
[2] Y. Katoh, T. Nozawa, A.M. Williams, T. Cheng, P. Dou, L.L. Snead, Properties of Hi-Nicalon Type-S CVI SiC Composite Irradiated to 70 dpa at Elevated Temperatures, ORNL/TM–2012/459, in, Oak Ridge National Laboratory, 2012.