Publisher Correction to: Welding in the World

https://doi.org/10.1007/s40194-020-01046-3

Due to a mistake during production the publication of this article unfortunately contained a mistake. Figure 10 was not correct, please see the correct Fig. 10 below.

Fig. 10
figure 1

Pulsed laser weld microstructural map, from [12]. The red line represents the range of solidification rates experienced by the 304 welds at the centerline. The blue line represents the range of solidification rates experienced by the 304 L welds at the centerline

The original article has been corrected.