Monomer release from bulk-fill composite resins in different curing protocols
Pinar GulHamit H. AlpMutlu Özcan
Author information
JOURNAL FREE ACCESS

2020 Volume 62 Issue 3 Pages 288-292

Details
Abstract

The purpose of this study was to determine the depth of cure and the type and amount of monomers released from bulk-fill composites in different curing protocols. Five different composite resins Filtek Bulk-Fill Posterior, Filtek Bulk-Fill Flowable, SureFil SDR, X-tra Fil, and X-tra base, were used. A light-emitting diode (LED) device was used in 3 different modes (standard, high power, and extra power mode), and a halogen light device was also used as a control. Surface hardness was measured and the depth of cure was calculated. Monomer analysis was performed using high performance liquid chromatography (HPLC). The data were analyzed using Tamhane’s T2 post-hoc test (α = 0.05). The cure depth for all materials except for Filtek Bulk-Fill Posterior (extra power mode) and Filtek Bulk-Fill Flowable (high power and extra power modes) was over 80%. Under the conditions of this study, the amount of monomer released from composite resins changed according to the type of composite resin and the light mode used.

Content from these authors
© 2020 by Nihon University School of Dentistry
Previous article Next article
feedback
Top