Characterization of aluminum-based coatings after short term exposure during irradiation campaign in the LVR-15 fission reactor
Fusion Engineering and Design ( IF 1.7 ) Pub Date : 2021-04-02 , DOI: 10.1016/j.fusengdes.2021.112521
Roman Petráš , Klára Kunzová , Alica Fedoriková , Jaroslav Kekrt , Michal Kordač , Fabio Di Fonzo , Boris Paladino , Carsten Schroer , Julia Lorenz , Marco Utili , Ladislav Vála

Protective aluminum-based coatings represent a promising anti-permeation and anti-corrosion barrier for breeding blanket systems developed for European DEMO fusion reactor. Following the prior in-depth characterizations, selected coating candidates were subjected to a combined test consisting of contact with liquid Pb-16Li, its repeated in-situ solidification and re-melting, tritium permeation during gamma and neutron irradiation in the LVR-15 fission reactor. During the sample exposure in the reactor, the temperature of Pb-16Li was between 300 and 425 °C. The irradiation damage averaged over the sample volume estimated by FISPACT code was limited to 0.037 dpa. This article presents post-irradiation characterization of cylindrical Eurofer97 samples coated by electro-chemical X-metal deposition from ionic liquid (ECX) and pulsed laser deposition (PLD) techniques. The coating damage relative to a reference uncoated sample is discussed.



中文翻译:

LVR-15裂变反应堆在辐照过程中短期暴露后对铝基涂层的表征

铝基保护涂层代表了为欧洲DEMO聚变反应堆开发的育种毯系统的有希望的防渗透和防腐蚀屏障。根据先前的深入表征,对选定的涂层候选物进行组合测试,包括与液态Pb-16Li接触,其反复原位固化和重熔,在LVR-15裂变中的γ辐射和中子辐照期间的ium渗透反应堆。在反应器中暴露样品期间,Pb-16Li的温度在300至425°C之间。通过FISPACT代码估算的样品体积的平均辐射损伤被限制在0.037 dpa。本文介绍了通过离子液体的电化学X-金属沉积(ECX)和脉冲激光沉积(PLD)技术涂覆的圆柱形Eurofer97样品的辐照后表征。讨论了相对于参考未涂层样品的涂层损伤。

更新日期:2021-04-04