Noble-metal-free catalysts based on apatite-type lanthanum silicate for complete toluene combustion
Functional Materials Letters ( IF 1.3 ) Pub Date : 2020-09-03 , DOI: 10.1142/s1793604720500356 Kenji Matsuo 1 , Naoyoshi Nunotani 1 , Nobuhito Imanaka 1
Functional Materials Letters ( IF 1.3 ) Pub Date : 2020-09-03 , DOI: 10.1142/s1793604720500356 Kenji Matsuo 1 , Naoyoshi Nunotani 1 , Nobuhito Imanaka 1
Affiliation
Noble-metal-free LaCoO3 /La[Formula: see text]Si5 CoO[Formula: see text]/[Formula: see text]-Al2 O3 catalysts were developed for complete toluene combustion, and their catalytic activities were investigated. The active oxygen supply from the apatite-type La[Formula: see text]Si5 CoO[Formula: see text] promoter successfully improved the oxidation ability of the LaCoO3 activator, and the highest catalytic activity was obtained for the 10 wt.% LaCoO3 /20 wt.% La[Formula: see text]Si5 CoO[Formula: see text]/[Formula: see text]-Al2 O3 catalyst, which oxidized toluene completely at the temperature as low as 300[Formula: see text]C.
中文翻译:
基于磷灰石型硅酸镧的无贵金属催化剂用于甲苯完全燃烧
无贵金属 LaCoO3 /La[公式:见正文]Si5 CoO[公式:见正文]/[公式:见正文]-Al2 ○3 开发了甲苯完全燃烧的催化剂,并研究了它们的催化活性。磷灰石型La的活性氧供给[公式:见正文]Si5 CoO[公式:见正文]促进剂成功提高了LaCoO的氧化能力3 活化剂,并且对于 10 wt.% LaCoO 获得最高的催化活性3 /20 wt.% La[公式:见正文]Si5 CoO[公式:见正文]/[公式:见正文]-Al2 ○3 催化剂,在低至300℃的温度下完全氧化甲苯[公式:见正文]C。