The Effect of Calcium Carbonate on the Photo‐Oxidative Behavior of Poly(butylene adipate‐co‐terephthalate)
Macromolecular Materials and Engineering ( IF 3.9 ) Pub Date : 2020-08-11 , DOI: 10.1002/mame.202000358
Vincenzo Titone 1 , Francesco Paolo La Mantia 1, 2 , Maria Chiara Mistretta 1
Affiliation  

The aim of this work is to evaluate the influence of nanosized CaCO3 on the photo‐oxidation of poly(butylene adipate‐co‐terephthalate) (PBAT)‐based nanocomposites. The PBAT/CaCO3 nanocomposites are prepared by using a corotating twin‐screw extruder with 0, 2, and 5 wt% of CaCO3. The films are obtained by film blowing process. Specimens of the nanocomposites and that of the pure polymer are subjected to accelerated aging with a cycle of 8 h of light at a temperature of 55 °C followed by 4 h condensation at 45 °C to evaluate the effects of the CaCO3 addition on the photo‐oxidation of PBAT. The results indicate that the modulus and tensile strength of the nanocomposites are increased significantly after incorporation of nanosized CaCO3, but, however, the elongation at break remains almost unchanged. The presence of the calcium carbonate slightly increases the photo‐oxidation rate of the matrix due to the presence of a stearate coating.

中文翻译:

碳酸钙对聚己二酸丁二醇酯-对苯二甲酸对苯二甲酸酯的光氧化行为的影响

这项工作的目的是评估纳米碳酸钙的影响3上的聚(亚丁基己二酸酯的光氧化-terephthalate)(PBAT)系纳米复合材料。PBAT / CaCO 3纳米复合材料是通过使用具有0、2和5 wt%的CaCO 3的同向双螺杆挤出机制备的。所述膜通过吹膜工艺获得。纳米复合材料的样品和纯聚合物的样品在55°C的温度下经过8 h的光循环加速老化,然后在45°C下冷凝4 h以评估CaCO 3的作用另外对PBAT的光氧化作用。结果表明,纳米复合CaCO 3掺入后,纳米复合材料的模量和拉伸强度显着提高,但是,断裂伸长率几乎保持不变。由于存在硬脂酸盐涂层,碳酸钙的存在会稍微增加基质的光氧化速率。