Cover Image, Volume 101, Issue 3
Journal of the American Ceramic Society ( IF 3.9 ) Pub Date : 2018-01-02 , DOI: 10.1111/jace.15131


Optical fractography of two samples of S200H tested under the same conditions (1473K, 265 MPa) showing different fracture morphologies. The sample (top) with a shorter life of 2.3h exhibits short pullout lengths while the sample (bottom) with a longer life of 20h runout and tested at RT exhibits a more fibrous fracture. DOI: 10.1111/jace.15131
image


中文翻译:

封面图片,第101卷,第3期

在相同条件下(1473K,265 MPa)测试的两个S200H样品的光学断口图显示出不同的断裂形态。寿命短于2.3h的样品(顶部)显示出较短的拔出长度,而寿命长20h的样品(底部)在室温下测试并显示出更多的纤维断裂。DOI:10.1111 / jace.15131