Stabilization of novel high temperature phase yellow-emitting σ-type (Ba1−x−yEuxMgy)2P2O7 phosphors using a melt synthesis technique
Inorganic Chemistry Frontiers ( IF 7 ) Pub Date : 2017-07-28 00:00:00 , DOI: 10.1039/c7qi00359e
H. Nakagawa 1, 2, 3, 4 , S. W. Kim 5, 6, 7, 8, 9 , T. Hasegawa 1, 2, 3, 4, 10 , S. Hasegawa 1, 2, 3, 4 , T. Ishigaki 1, 2, 3, 4 , K. Uematsu 1, 2, 3, 4 , K. Toda 1, 2, 3, 4 , H. Takaba 4, 11, 12, 13, 14 , M. Sato 2, 3, 4, 15
Affiliation  

Novel Eu2+-activated phosphate phosphors based on high-temperature phase σ-Ba2P2O7, which is an unstable phase at room temperature, were synthesized for the first time by a melt synthesis technique using an arc-imaging furnace. By doping Mg2+ into the host lattice, Eu2+-activated σ-Ba2P2O7 phosphors were successfully obtained in a single phase form of a hexagonal structure and the emission intensity was also effectively enhanced. The relative emission peak intensity of the σ-(Ba0.67Eu0.03Mg0.30)2P2O7 phosphor was 315% of that for the σ-(Ba0.97Eu0.03)2P2O7 phosphor. The emission color tunable from green emission with a peak at 516 nm to yellow emission with a peak at 551 nm can be achieved by controlling the Mg2+ content in the σ-(Ba0.97−yEu0.03Mgy)2P2O7 phosphors.

中文翻译:

利用熔融合成技术稳定新型高温相发射黄光的σ型(Ba 1 - x - y Eu x Mg y2 P 2 O 7荧光粉

新颖的Eu 2+基于高温相σ钡活化磷酸盐荧光2 P 2 ö 7,其是在室温下不稳定的阶段,通过使用电弧成像炉的熔融合成技术首次合成。通过掺杂的Mg 2+到主晶格,铕2+ -activatedσ钡2 P 2个ö 7以六边形结构的单相形式被成功得到的荧光体和发光强度也有效地提高。σ-(Ba 0.67 Eu 0.03 Mg 0.302 P的相对发射峰强度2 O 7荧光粉为σ-(Ba 0.97 Eu 0.03 2 P 2 O 7荧光粉的315%。可以通过控制σ-(Ba 0.97- y Eu 0.03 Mg y 2 P 2 O中的Mg 2+含量,实现从516 nm峰的绿色发射到551 nm峰的黄色发射可调的发射颜色。 7种荧光粉。